| Truing and Dressing |
| If the periphery runout is severe when the grinding wheel is mounted, or if profile wear of the straight wheel or cup wheel is found, the runout and profile of the wheel must be adjusted. |
| |
| Truing is the procedure of adjusting the runout and profile of the wheel. If involves shaving off the diamond grits and the bond to correct the runout and the profile of the wheel. |
| |
| The diamond grinding wheel cannot be use immediately after the turing procedure as the diamond grits are not properly exposed: therefore, the wheel is not in prime condition to be used. |
| |
| To improve free-cutting ability, the bond must be dug out and the diamond grits exposed onto the surface of the wheel. This process is called "Dressing". |
| |
| Diamond grinding wheels cannot satisfactorily perform unless the above procedures are followed correctly. |
| |
| |
| Selection of Silicon Carbide Wheel for Truing |
| In order for the truing of the diamond grinding wheel to be effectively performed a timely manner, the grit size of the silicon carbide truing wheel must be 2 grades coarser than that of the diamond grinding wheel. As shown below, the grade of the silicon carbide wheel must be relatively hard. |